FCC Workgroup #3 – Refractory

Home Forums Conferences 2013 CatCracking Texas FCC Workgroup #3 – Refractory

Viewing 0 reply threads
  • Author
    Posts
    • #1654
      Anonymous
      Guest

      SME facilitators –
      Damon McCrory, Harbison-Walker Refractories Co & Barry Robinson, Middough
       
      Refractory Failure
      Between FGSV & orifice chamber
      At 1100-1200F on steel OD
      Failed after 1 year
      Look at process conditions, refractory type, vendor, anchors
      Dryout Temps
      300 F with hold
      600-700 F with hold
      1000- 1200 F with hold
      24 hr air cure important
      HIS: jave hydrotested lined vessels with curing afterward
      Structure tours: once every 2 hours with cold marked.